SA335 P5c superalloy pipe material

 Maybe you have heard of P5 grade seamless pipe, so have you heard of P5c grade seamless pipe? P5c grade high temperature seamless pipe is a ferritic alloy steel material according to ASME SA335 standard. It can be used in high temperature environment. The chemical elements contained in the material make P5c have good deformation ability, plasticity, weldability, hardenability, etc., and can maintain good working ability even in high temperature environment.

CHEMICAL COMPOSITION OF ALLOY STEEL P5c PIPES

Grade P5c
C, %
Mn, %
P, %
S, %
Si, %
Cr, %
Mo, %
UNS K41245
0.12 max
0.30-0.60
0.025 max
0.025 max
0.5 max
4.00-6.00
0.45-0.65
 

MECHANICAL PROPERTIES OF ALLOY STEEL P5c PIPES

Tensile Strength, MPa
Yield Strength, MPa
Elongation, %
415 min
205 min
30 min

P5c high temperature seamless pipes are mostly used in petroleum miners, industrial buildings, pressure vessel pipes and other industries. Compared to the P5 grade, the carbon content is reduced. The delivery temperature range for heat treatment should be 715-745°C.

If you want to buy alloy steel pipes for high temperature, but don't know which material to choose, you can consult us.


From:http://boilersteelpipe.com/pro/smls/sa335-p5c-superalloy-pipe-material.html

评论

此博客中的热门博文

What are the surface treatments of EN 10294-1 E355+N seamless pipes

What are the usual pipes for Power Generation Boiler?

What are the applications of steel pipes in the automobile manufacturing industry?