Delivery status of SA335 P5b superalloy pipe

 SA335 P5b grade is one of the grades of ASME SA335 Standard Specification for Ferritic Seamless Alloy Pipe for High Temperature Environment. This grade is mainly used in petrochemical gas industry and some other construction industries.

CHEMICAL COMPOSITION OF ALLOY STEEL P5b PIPES

Grade P5b
C, %
Mn, %
P, %
S, %
Si, %
Cr, %
Mo, %
UNS K51545
0.15 max
0.30-0.60
0.025 max
0.025 max
1.00-2.00
4.00-6.00
0.45-0.65
 

MECHANICAL PROPERTIES OF ALLOY STEEL P5b PIPES

Tensile Strength, MPa
Yield Strength, MPa
Elongation, %
415 min
205 min
30 min

SA335 P5b seamless pipe can be made by hot working or cold drawing process, and should be reheated and supplied in fully annealed, isothermal annealed or normalized and tempered condition. If it is supplied in normalized and tempered state, the minimum tempering temperature of P5b grade pipe should be 675℃.

Do you need ASME SA335 P5b superalloy pipe? If yes, please feel free to contact us for the latest quotation.

From:http://boilersteelpipe.com/pro/smls/delivery-status-of-sa335-p5b-superalloy-pipe.html

评论

此博客中的热门博文

What are the surface treatments of EN 10294-1 E355+N seamless pipes

What are the usual pipes for Power Generation Boiler?

What are the applications of steel pipes in the automobile manufacturing industry?